Foshan Guangyuan Technology Co., Ltd.
Products
Contact Us
  • Contact Person : Mr. Du Nick
  • Company Name : Foshan Guangyuan Technology Co., Ltd.
  • Tel : 86-757-85438329
  • Fax : 86-757-85438329
  • Address : Guangdong,Foshan,XingZhongDa Industrial Zone, Luohang, Jinsha, Danzao, Nanhai, Foshan
  • Country/Region : China
  • Zip : China

Alkaline Copper Cyanide Plating Chemicals for Button, Zipper, Lighting

Alkaline Copper Cyanide Plating Chemicals for Button, Zipper, Lighting
Product Detailed
Related Categories:Other Chemicals
Alkaline Copper Plating Chemicals for Button, Zipper, Lighting low cost and easy operate. cyanide type

Alkaline Cyanide Copper Plating Chemicals for button, zipper, buckle

1. Features

1.Bright and smooth coating, the crystallization of dense, small gap;

2. Wide range of current density, excellent coverage;

3. Impurities in high-tolerance, easy to control;

4.Selected to use in basic parts of different material, especially for zinc alloy die castings;

5. You can use Sodium salt to make up plating solution, low-cost.

Widely applied in the base copper plating, for garment accessories like zipper, button, buckle

2. The component of the plating solution

Materials

Make-up volume

Zinc alloy

Iron parts

Cuprous cyanide

45-65g/L

35-50g/L

Sodium cyanide

66-93g/L

52-70g/L

Sodium hydroxide

1-3g/L

10-20g/L

Neochel

30-50ml/L

30-50ml/L

CuppA3# L-3 brightener

5-7mlL

5-7ml/L

CuppA3# L-4 auxiliary agent

5ml/L

5ml/L

3. Work Conditions

Operating parameters

Standard volume

Zinc alloy

Iron parts

Copper metal

32-46g/L

35-50g/L

Free sodium cyanide

17-22g/L

13-20g/L

Sodium hydroxide

1-3g/L

10-20g/L

temperature

50-65°C

45-55°C

Current density

2-5   AMP/DM2

2   AMP/DM2

agitate

Air agitate and cathode swing

Air agitate and cathode swing

anode

Pure copper

Pure copper

Anode bag

necessary

necessary

filtering

Continuous filtering

Continuous filtering

4. Solution Preparation:

1. Fill the clean tank with 2/3 full of deionised water and then heat to about 50°C;

2. Add required quantity of the potassium/sodium hydroxide; stir to get it dissolve completely. Add required Neochel or sodium cyanide, stir further to get it dissolve completely.

3. Add the required cuprous cyanidewith vigorous stirring to get it dissolve completely;

4. Add 4-6g/L activated carbon, stir the solution continuously for about two hours and then let it stay for above four hours or a whole night.

5. Filter the plating solution into a clean plating tank with a filtering pump;

6. Add the water to required volume;

7. Electrolyze the solution for about 4-8 hours by low current density (0.5 AMP/ DM2) with wave-shaped stainless steel cathode;

8. Add the additives and stir the solution thoroughly, heat it to working temperature and operate the bath.

  

widely applied in plating industries, for the base copper layer, with good quality and easy operation.

Alkaline Copper Cyanide Plating Chemicals for Button, Zipper, Lighting



Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.